Solutions for Crack Problems at Weld Inlet of Condenser
The crack at the inlet end of the condenser weld is mainly characterized by brittle cracking. The crack originates from the upper end of the tooth-shaped plate. The crack cracks along the grain. The main morphological feature is cleavage intergranular secondary cracking, which has the characteristics of stress corrosion cracking. This is because the exit end weld bears large welding residual stress and thermal stress, and is affected by the high-mass fraction of chloride ions in the medium and high temperature. Chloride stress corrosion cracking occurs. There is a temperature difference between the compression plate and the plate bundle. If the temperature difference reaches 100e, the temperature difference stress generated on the compression plate is greater than the standard yield strength of the 304 material. In addition, the thickness of the tube plate in the original structure of
Condenser is 60mm, and the outer edge of the tube plate is limited by the diameter of the shell.
Solution:
1. Disconnect the compression plate, and add an upper expansion joint to the insulating ladder to absorb the expansion difference between the plate bundle and the compression plate. The tube-sheet structure is cancelled, and the same dome cover as the lower part of the plate bundle is added to the upper part of the plate bundle, which can reduce some expansion constraints in the width direction of the plate.
The mass of the plate bundle is borne by the newly installed tube plate, and the condenser tube plate is clamped by the equipment flange. Set support beams on the end faces of the plate bundles. Crack treatment reduces the channel length of the inlet and outlet of the plate bundle shell to improve the heat transfer effect.