Impact of Iron Oxide Scale on Tube Condenser
Iron oxide scale The reason for the generation of iron oxide scale is that the tubes are sometimes empty and sometimes filled with water after outage, coupled with the erosion of condensate water after the shell-side oil is heated at 30~4O°℃, resulting in the existence of a rust layer and accelerated corrosion. This direct chemical reaction between the chemical medium and the metal produces a large amount of iron oxide scale and causes equipment damage. This phenomenon is very common in
tube condensers.
If protection is not strengthened, the service life of the equipment will be greatly shortened. In severe cases, the entire equipment will be scrapped in a short time, causing economic losses.